The correct option is (b) 50 to 140
To explain I would say: In squeeze casting, the punch portion of the upper die is forced into the cavity by displacing the molten metal under pressure until it fills the annular space between the die and the punch. Normally, the metal is kept under pressure of 50 to 140 MPa to avoid the formation of shrinkage defects.