Which of the following corrosion test is most reliable to know the extent of pitting corrosion?

(a) To measure the average depth of pits

(b) To measure the maximum depth of a pit

(c) Weight loss method

(d) Weight gain method

I had been asked this question in quiz.

I'm obligated to ask this question of Eight Forms in division Eight Forms of Corrosion of Corrosion Engineering

1 Answer

+1 vote
by (888k points)
selected by
 
Best answer
Right option is (b) To measure the maximum depth of a pit

The best I can explain: The measurement of maximum depth of pit would be a more reliable way of expressing pitting corrosion. As metal loss or metal gain (corrosion product) is very small and does not indicate the depth of penetration.

Related questions

Welcome to TalkJarvis QnA, a question-answer community website for the people by the people. On TalkJarvis QnA you can ask your doubts, curiosity, questions, and whatever is going through your mind, either related to studies or others. Experts and people from different fields will answer.

Find easy, practical guides for smarter living in Japan. Visit Mikataa (Japanese) and The Japanese Ways (English) for simple tips, lifestyle insights, and everyday know-how, along with EV Pulse

Most popular tags

biology – class 12 biology – class 11 construction & building materials chemistry – class 12 electronic devices & circuits network theory data structures & algorithms ii cell biology ic engine insurance finance money computational fluid dynamics engineering physics i discrete mathematics chemistry – class 11 aerodynamics casting-forming-welding i engineering mathematics operating system casting-forming-welding ii engineering drawing mysql engineering geology digital circuits wireless mobile energy management electrical measurements digital communications cyber security analytical instrumentation embedded systems electric drives cytogenetics advanced machining computer fundamentals life sciences basic civil engineering iot design of electrical machines physics – class 12 applied chemistry dairy engineering basic chemical engineering cloud computing microprocessor bioinformatics aircraft design aircraft maintenance software engineering drug biotechnology digital signal processing biochemistry data structures & algorithms i automotive engine design avionics engineering material & metallurgy energy engineering cognitive radio unix electrical machines biomedical instrumentation object oriented programming electromagnetic theory power electronics analog communications bioprocess engineering civil engineering drawing engineering metrology physics – class 11 mathematics – class 12 engineering chemistry i basic electrical engineering unit processes mongodb signals and systems cryptograph & network security hadoop mathematics – class 11 engineering physics ii html control systems engineering mechanics antennas analog circuits computer network java sql server javascript concrete technology chemical process calculation artificial intelligence design of steel structures c++ database management computer architecture engineering chemistry ii corrosion engineering chemical technology dc machines
...