Right option is (d) Titanium and martensitic iron-base alloys
The best I can explain: Hydrogen embrittlement refers to the brittle cracking failure of reactive metals due to the formation of metal hydrides. Titanium, ferritic, and martensitic iron-base alloys are susceptible to hydrogen embrittlement.