Right option is (a) Heated 30-60^oC above A1 line
To explain: Hypoeutectoid steels are heated above the A3 line and then cooled in the furnace. On the other hand, hypereutectoid steels are heated 30-60^oC above the A1 line and then cooled similar to hypoeutectoid steels.