Right choice is (b) 0.25 mm
Explanation: Of all the diffusion surface hardening methods, carburizing provides the highest cast depth of 1.38 mm. This is followed by carbonitriding, nitriding, and cyaniding at 0.5 mm, 0.38 mm, and 0.25 mm correspondingly.